Description
The 8000 Series offers the highest glass transition temperature and the highest degree of crystallinity, leading to the best tensile and compression strengths among the wide range of PEKK copolymers within the KEPSTAN product range.
KEPSTAN 8000 Series includes a low flow grade, KEPSTAN 8001, and a medium flow grade, KEPSTAN 8002, both unfilled pure PEKK resins designed to meet the requirements of a broad range of melt processing technologies, including among others extrusion of stock shapes, tubes, films, extrusion compression, compression molding, injection molding of thick or complex and thin-walled parts.
Arkema Kepstan 8001
Arkema Kepstan 8002
KEPSTAN PEKK resin is available in pellet form and in powder form with different particle sizes.
Standard packaging includes 20 kg boxes for pellets and 10 kg boxes for powders.
Other information
Drying temperature and time: 150°C for 3 to 4 hours or 120°C for 6 to 8 hours
Processing temperature: 375 - 385°C
Temperature settings - Injection: Rear 350°C / Center 375°C / Front 375°C / Nozzle 385°C
Mold temperature (to facilitate filling of the cavity and polymer crystallization): 220 - 240°C
Temperature settings - Extrusion: Zones 1/2/3/4: 340°C/ 360°C/ 380°C/ 380°C Die: 370°C